liu kai, du kai, chen jing, et al. Fabrication of high quality ordered porous anodic aluminum oxide templates[J]. High Power Laser and Particle Beams, 2010, 22.
Citation:
liu kai, du kai, chen jing, et al. Fabrication of high quality ordered porous anodic aluminum oxide templates[J]. High Power Laser and Particle Beams, 2010, 22.
liu kai, du kai, chen jing, et al. Fabrication of high quality ordered porous anodic aluminum oxide templates[J]. High Power Laser and Particle Beams, 2010, 22.
Citation:
liu kai, du kai, chen jing, et al. Fabrication of high quality ordered porous anodic aluminum oxide templates[J]. High Power Laser and Particle Beams, 2010, 22.
The preparation of porous anodic aluminum oxide (AAO) templates has been studied with oxalic acid as electrolyte. The morphology of the as-prepared templates has been characterized by field-emission scanning electron microscope (FE-SEM). The pores distributed orderly and uniformly with the diameter ranging from 40 nm to 70 nm. The experimental results indicate that electrolyte concentration, oxidation voltage, oxidation temperature and oxidation time affect the structure of AAO templates. Ordered porous AAO templates can be derived without annealing and finishing. X-ray diffraction (XRD) analysis indicates that the aluminum oxide film is mainly composed of amorphous Al2O3/sub>.